“ISO 20480:2021 Fine bubble technology – General principles for usage and measurement of fine bubbles – Part 3: Methods for generating fine bubbles” has been added to your cart. View cart

ISO 11463:2020
ISO 11463:2020 Corrosion of metals and alloys – Guidelines for the evaluation of pitting corrosion
CDN $115.00
SKU: 1f95f25c6f1d
Categories: ICS:77.060, SUSTAINABLE_DEVELOPMENT_GOAL:15, SUSTAINABLE_DEVELOPMENT_GOAL:6, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.
Edition
2
Published Date
2020-08-06
Status
PUBLISHED
Pages
12
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 10263:2009 Earth-moving machinery – Operator enclosure environment – Part 1: Terms and definitions
0 out of 5CDN $76.00 Add to cart -
ISO 21120:2025 Machinery for forestry – Forestry mulching equipment – Terms, definitions and commercial specifications
0 out of 5CDN $173.00 Add to cart -
ISO 1991:1982 Vegetables – Nomenclature – First list
0 out of 5CDN $115.00 Add to cart -
ISO 5157:2023 Textiles – Environmental aspects – Vocabulary
0 out of 5CDN $76.00 Add to cart