REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 23.2: Reconciliation of Liquid Tank Car(s) Quantities : Reaffirmed

$

218

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 16A: Specification for Drill-through Equipment

$

322

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-2: Field Testing Oil-based Drilling Fluids wA1

$

388

BUY NOW

ISO 15607:2019

ISO 15607:2019 Specification and qualification of welding procedures for metallic materials – General rules

CDN $115.00

SKU: da1e3c4c2453 Category:

Description

This document is part of a series of standards dealing with specification and qualification of welding procedures. Annex A gives details of this series of standards, Annex B gives a table for the use of these standards, and Annex C gives a flow diagram for the development and qualification of a WPS.

This document defines general rules for the specification and qualification of welding procedures for metallic materials. This document also refers to several other standards as regards detailed rules for specific applications.

This document is applicable to manual, partly mechanized, fully mechanized and automated welding.

Welding procedures are qualified by conforming to one or more welding procedure qualification records (WPQR). The use of a particular method of qualification is often a requirement of an application standard.

It is assumed that welding procedure specifications are used in production by competent welders, qualified in accordance with the relevant part of ISO 9606 or by competent operators qualified in accordance with ISO 14732.

Edition

2

Published Date

2019-10-07

Status

PUBLISHED

Pages

10

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

This document is part of a series of standards dealing with specification and qualification of welding procedures. Annex A gives details of this series of standards, Annex B gives a table for the use of these standards, and Annex C gives a flow diagram for the development and qualification of a WPS.

This document defines general rules for the specification and qualification of welding procedures for metallic materials. This document also refers to several other standards as regards detailed rules for specific applications.

This document is applicable to manual, partly mechanized, fully mechanized and automated welding.

Welding procedures are qualified by conforming to one or more welding procedure qualification records (WPQR). The use of a particular method of qualification is often a requirement of an application standard.

It is assumed that welding procedure specifications are used in production by competent welders, qualified in accordance with the relevant part of ISO 9606 or by competent operators qualified in accordance with ISO 14732.