Your cart is currently empty!

ISO 16260:2016
ISO 16260:2016 Paper and board – Determination of internal bond strength
CDN $173.00
Description
ISO 16260:2016 describes a method to measure the energy required to rapidly delaminate a test piece of paper or board. Rupture of the test piece in the “Z” or thickness direction is initiated by a pendulum having a defined mass, moving at a defined velocity.
The procedure is suitable for both single- and multi-ply papers and boards, including coated sheets and those that are laminated with synthetic polymer films. It is particularly suitable for papers and boards that may be subjected to Z-direction[2],[5] rapid impacts, impulses, or shock loads during printing or conversion.
The test procedure entails the adherence of double-sided adhesive tape to both sides of the test piece under pressure. For this reason, the method may be unsuitable for materials that might be structurally damaged by compression or are porous enough to permit migration of the tape adhesive into or through the test piece.
Edition
1
Published Date
2016-05-25
Status
PUBLISHED
Pages
15
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
ISO 16260:2016 describes a method to measure the energy required to rapidly delaminate a test piece of paper or board. Rupture of the test piece in the "Z" or thickness direction is initiated by a pendulum having a defined mass, moving at a defined velocity.
The procedure is suitable for both single- and multi-ply papers and boards, including coated sheets and those that are laminated with synthetic polymer films. It is particularly suitable for papers and boards that may be subjected to Z-direction[2],[5] rapid impacts, impulses, or shock loads during printing or conversion.
The test procedure entails the adherence of double-sided adhesive tape to both sides of the test piece under pressure. For this reason, the method may be unsuitable for materials that might be structurally damaged by compression or are porous enough to permit migration of the tape adhesive into or through the test piece.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 4046:2016 Paper, board, pulps and related terms – Vocabulary – Part 1: Alphabetical index
0 out of 5CDN $76.00 Add to cart -
ISO 3036:2025 Board – Determination of puncture resistance using a pendulum device
0 out of 5CDN $115.00 Add to cart -
ISO 8784:2023 Pulp, paper and board – Microbiological examination – Part 2: Enumeration of bacteria, yeast and mould on surface
0 out of 5CDN $76.00 Add to cart -
ISO 4046:2016 Paper, board, pulps and related terms – Vocabulary – Part 5: Properties of pulp, paper and board
0 out of 5CDN $76.00 Add to cart