Your cart is currently empty!

ISO 20728:2018
ISO 20728:2018 Corrosion of metal and alloys – Determination of resistance of magnesium alloys to stress corrosion cracking
CDN $115.00
Description
This document specifies a method for the determination of resistance to stress corrosion cracking (SCC) of magnesium alloys intended for use in structural applications (such as magnesium front end, gearbox and clutch housing units, steering column parts, shift actuators, valve covers and housings, brackets and intake manifold blades, electronic devices, power tools and medical equipment). The method allows determination of the resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of magnesium alloys.
The document is applicable to cast and wrought magnesium alloys in the form of castings, semi-finished products, parts and weldments and covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.
The document allows assessment of the relative performance of materials and products in environments containing chlorides or sulphates, provided that the failure mechanism is not changed, but does not qualify a material or product for service application.
Edition
1
Published Date
2018-09-05
Status
PUBLISHED
Pages
12
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies a method for the determination of resistance to stress corrosion cracking (SCC) of magnesium alloys intended for use in structural applications (such as magnesium front end, gearbox and clutch housing units, steering column parts, shift actuators, valve covers and housings, brackets and intake manifold blades, electronic devices, power tools and medical equipment). The method allows determination of the resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of magnesium alloys.
The document is applicable to cast and wrought magnesium alloys in the form of castings, semi-finished products, parts and weldments and covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.
The document allows assessment of the relative performance of materials and products in environments containing chlorides or sulphates, provided that the failure mechanism is not changed, but does not qualify a material or product for service application.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 5053:2019 Industrial trucks – Vocabulary – Part 2: Fork arms and attachments
0 out of 5CDN $351.00 Add to cart -
ISO 8384:2019 Ships and marine technology – Dredgers – Vocabulary
0 out of 5CDN $76.00 Add to cart -
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 7: Diagnostics and therapeutics for healthcare
0 out of 5CDN $115.00 Add to cart