ISO 23228:2011
ISO 23228:2011 Thermoplastics pipes for the conveyance of fluids – Determination of the stress-rupture resistance of moulding materials using plain strain grooved tensile (PSGT) specimens
CDN $115.00
Description
ISO 23228:2011 specifies a method for the determination of the time-to-failure of thermoplastics resins and compounds for piping and fitting applications by the use of a plane strain grooved tensile specimen in a stress-rupture test.
The grooved tensile specimen produces a biaxial state of stress on uni-axial loading, which is taken to be indicative of the stress conditions found in pressurized solid-wall plastics pipes. The ratio of the stress in the axial direction to the transverse direction approximates that for a pressurized end-capped solid-wall pipe specimen.
It is intended that the data generated on these specimens be utilized to determine the stress-rupture (time-to-failure) resistance of moulding materials for pipes and fittings as well as experimental piping resins.
This method is also applicable to stress-rupture evaluations of pipes which are difficult to test, e.g. larger diameter pipes, including their batch release tests.
ISO 23228:2011 is not intended to replace the stress-rupture test of ISO 1167, which uses internally pressurized end-capped pipes.
Edition
1
Published Date
2011-09-29
Status
PUBLISHED
Pages
9
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
ISO 23228:2011 specifies a method for the determination of the time-to-failure of thermoplastics resins and compounds for piping and fitting applications by the use of a plane strain grooved tensile specimen in a stress-rupture test.
The grooved tensile specimen produces a biaxial state of stress on uni-axial loading, which is taken to be indicative of the stress conditions found in pressurized solid-wall plastics pipes. The ratio of the stress in the axial direction to the transverse direction approximates that for a pressurized end-capped solid-wall pipe specimen.
It is intended that the data generated on these specimens be utilized to determine the stress-rupture (time-to-failure) resistance of moulding materials for pipes and fittings as well as experimental piping resins.
This method is also applicable to stress-rupture evaluations of pipes which are difficult to test, e.g. larger diameter pipes, including their batch release tests.
ISO 23228:2011 is not intended to replace the stress-rupture test of ISO 1167, which uses internally pressurized end-capped pipes.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 5053:2019 Industrial trucks – Vocabulary – Part 2: Fork arms and attachments
0 out of 5CDN $351.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart -
ISO 5078:2025 Management of terminology resources – Terminology extraction
0 out of 5CDN $233.00 Add to cart -
ISO 10110:2019 Optics and photonics – Preparation of drawings for optical elements and systems – Part 1: General
0 out of 5CDN $312.00 Add to cart