REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 23.2: Reconciliation of Liquid Tank Car(s) Quantities : Reaffirmed

$

218

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 16A: Specification for Drill-through Equipment

$

322

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-2: Field Testing Oil-based Drilling Fluids wA1

$

388

BUY NOW

ISO 4589:2017

ISO 4589:2017 Plastics – Determination of burning behaviour by oxygen index – Part 3: Elevated-temperature test

CDN $233.00

Description

ISO 4589-3:2017 specifies methods for determining the minimum volume fraction of oxygen, in a mixture with nitrogen, that will support combustion of small vertical test specimens under specified test conditions over a range of temperatures between 25 °C and 150 °C. The range of temperatures is typically between 40 °C and 150 °C. The results are defined as temperature index values at the test temperature, which is typical of the practical temperature that a plastic material can experience in an overheated service situation.

Methods are provided for testing materials that are self-supporting at the test temperature in the form of vertical bars or sheet up to 10,5 mm thick. However, they are not applicable to form V which requires a supporting frame as defined in ISO 4589‚Äë2:2017, Table 2. These methods are suitable for solid, laminated or cellular materials characterized by an apparent density 100 kg/m3 or higher. The methods are also applicable to some cellular materials having an apparent density of less than 100 kg/m3. A method is provided for testing flexible sheet or film materials while supported vertically.

ISO 4589-3:2017 also includes a method (see Annex A) for determining the temperature at which the OI of small vertical test specimens in air is 20,9 % under specified test conditions. The temperature at which this occurs is defined as the flammability temperature (FT) and the method is limited to the determination of temperatures less than 400 °C. The method is not applicable to materials having an OI of <20,9 %.

Edition

2

Published Date

2017-04-12

Status

PUBLISHED

Pages

19

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 4589-3:2017 specifies methods for determining the minimum volume fraction of oxygen, in a mixture with nitrogen, that will support combustion of small vertical test specimens under specified test conditions over a range of temperatures between 25 °C and 150 °C. The range of temperatures is typically between 40 °C and 150 °C. The results are defined as temperature index values at the test temperature, which is typical of the practical temperature that a plastic material can experience in an overheated service situation.

Methods are provided for testing materials that are self-supporting at the test temperature in the form of vertical bars or sheet up to 10,5 mm thick. However, they are not applicable to form V which requires a supporting frame as defined in ISO 4589‚Äë2:2017, Table 2. These methods are suitable for solid, laminated or cellular materials characterized by an apparent density 100 kg/m3 or higher. The methods are also applicable to some cellular materials having an apparent density of less than 100 kg/m3. A method is provided for testing flexible sheet or film materials while supported vertically.

ISO 4589-3:2017 also includes a method (see Annex A) for determining the temperature at which the OI of small vertical test specimens in air is 20,9 % under specified test conditions. The temperature at which this occurs is defined as the flammability temperature (FT) and the method is limited to the determination of temperatures less than 400 °C. The method is not applicable to materials having an OI of <20,9 %.

Previous Editions