Your cart is currently empty!

ISO 7539:2020
ISO 7539:2020 Corrosion of metals and alloys – Stress corrosion testing – Part 10: Reverse U-bend method
CDN $173.00
SKU: d5c6fcc81aaa
Category: ICS:77.060
Description
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term “metal” as used in this document includes alloys.
Edition
2
Published Date
2020-05-12
Status
PUBLISHED
Pages
15
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term "metal" as used in this document includes alloys.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 11844:2020 Corrosion of metals and alloys – Classification of low corrosivity of indoor atmospheres – Part 1: Determination and estimation of indoor corrosivity
0 out of 5CDN $233.00 Add to cart -
ISO 17081:2014 Method of measurement of hydrogen permeation and determination of hydrogen uptake and transport in metals by an electrochemical technique
0 out of 5CDN $233.00 Add to cart -
ISO 22479:2019 Corrosion of metals and alloys – Sulfur dioxide test in a humid atmosphere (fixed gas method)
0 out of 5CDN $173.00 Add to cart -
ISO 18070:2015 Corrosion of metals and alloys – Crevice corrosion formers with disc springs for flat specimens or tubes made from stainless steel
0 out of 5CDN $115.00 Add to cart