ISO 7539:2013
ISO 7539:2013 Corrosion of metals and alloys – Stress corrosion testing – Part 11: Guidelines for testing the resistance of metals and alloys to hydrogen embrittlement and hydrogen-assisted cracking
CDN $173.00
SKU: 8e6ea89b780a
Categories: ICS:77.060, SUSTAINABLE_DEVELOPMENT_GOAL:11, SUSTAINABLE_DEVELOPMENT_GOAL:7, SUSTAINABLE_DEVELOPMENT_GOAL:9
Description
ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.
Edition
1
Published Date
2013-04-09
Status
PUBLISHED
Pages
16
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
ISO 7539-11:2013 gives guidance on the key features that should be accounted for in designing and conducting tests to evaluate the resistance of a metal or its alloy to hydrogen embrittlement and hydrogen-assisted cracking.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 2382:2015 Information technology – Vocabulary
0 out of 5CDN $0.00 Add to cart -
ISO 20537:2025 Footwear – Identification of defects during visual inspection – Vocabulary
0 out of 5CDN $273.00 Add to cart -
ISO 80004:2011 Nanotechnologies – Vocabulary – Part 5: Nano/bio interface
0 out of 5CDN $76.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart