ISO 7539:1989
ISO 7539:1989 Corrosion of metals and alloys – Stress corrosion testing – Part 3: Preparation and use of U-bend specimens
CDN $76.00
Description
Covers procedures for designing, preparing and using U-bend test specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, flat extruded material, wire or rod). The principal acvantages of the U-bend test are its simplicity and its adaptability for use in plants. A disadvantage is that stesses cannot be quantified with accuracy. U-bend specimens made from high strength materials may fracture rapidly and can be dangerous.
Edition
1
Published Date
1989-12-14
Status
PUBLISHED
Pages
3
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
Covers procedures for designing, preparing and using U-bend test specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, flat extruded material, wire or rod). The principal acvantages of the U-bend test are its simplicity and its adaptability for use in plants. A disadvantage is that stesses cannot be quantified with accuracy. U-bend specimens made from high strength materials may fracture rapidly and can be dangerous.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 80000:2019 Quantities and units – Part 11: Characteristic numbers
0 out of 5CDN $312.00 Add to cart -
ISO 80004:2020 Nanotechnologies – Vocabulary – Part 3: Carbon nano-objects
0 out of 5CDN $76.00 Add to cart -
ISO 80000:2025 Quantities and units – Part 13: Information science and technology
0 out of 5CDN $203.00 Add to cart