ISO 7539:1989 Corrosion of metals and alloys – Stress corrosion testing – Part 4: Preparation and use of uniaxially loaded tension specimens
CDN $76.00
Description
Covers procedures for designing, preparing and using uniaxially loaded tension specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, tubes, wire or rod as well as parts joined by welding, riveting, or other methods). Uniaxially loaded tensile specimens may be stressed quantitatively with equipment for application of either a constant load, a constant strain or an increasing load or strain.
Edition
1
Published Date
1989-12-07
Status
PUBLISHED
Pages
3
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
Covers procedures for designing, preparing and using uniaxially loaded tension specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, tubes, wire or rod as well as parts joined by welding, riveting, or other methods). Uniaxially loaded tensile specimens may be stressed quantitatively with equipment for application of either a constant load, a constant strain or an increasing load or strain.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 612:1978 Road vehicles – Dimensions of motor vehicles and towed vehicles – Terms and definitions
0 out of 5CDN $173.00 Add to cart -
ISO 1176:1990 Road vehicles – Masses – Vocabulary and codes
0 out of 5CDN $115.00 Add to cart -
ISO 20537:2025 Footwear – Identification of defects during visual inspection – Vocabulary
0 out of 5CDN $273.00 Add to cart -
ISO 80000:2025 Quantities and units – Part 13: Information science and technology
0 out of 5CDN $203.00 Add to cart