ISO 7539:1989
ISO 7539:1989 Corrosion of metals and alloys – Stress corrosion testing – Part 5: Preparation and use of C-ring specimens
CDN $115.00
Description
Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.
Edition
1
Published Date
1989-12-07
Status
PUBLISHED
Pages
9
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 22553:2019 Paints and varnishes – Electro-deposition coatings – Part 1: Vocabulary
0 out of 5CDN $76.00 Add to cart -
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 3833:1977 Road vehicles – Types – Terms and definitions
0 out of 5CDN $115.00 Add to cart -
ISO 14416:2003 Information and documentation – Requirements for binding of books, periodicals, serials and other paper documents for archive and library use – Methods and materials
0 out of 5CDN $273.00 Add to cart