ISO 7539:2005 Corrosion of metals and alloys – Stress corrosion testing – Part 7: Method for slow strain rate testing
CDN $115.00
Description
ISO 7539-7:2005 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure. The term “metal” as used in this part of ISO 7539 includes alloys.
Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.
The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.
Edition
2
Published Date
2005-02-04
Status
PUBLISHED
Pages
7
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
ISO 7539-7:2005 covers procedures for conducting slow strain rate tests for investigating susceptibility of a metal to stress corrosion cracking, including hydrogen-induced failure. The term "metal" as used in this part of ISO 7539 includes alloys.
Slow strain rate tests are adaptable for testing a wide variety of product forms, including plate, rod, wire, sheet and tubes, as well as composites of these and parts joined by welding. Notched specimens may be used, as well as initially plain specimens.
The principal advantage of the test is the rapidity with which susceptibility to stress corrosion cracking of a particular metal/environment combination can be assessed.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 8927:1991 Earth-moving machinery – Machine availability – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 80000:2019 Quantities and units – Part 11: Characteristic numbers
0 out of 5CDN $312.00 Add to cart -
ISO 3833:1977 Road vehicles – Types – Terms and definitions
0 out of 5CDN $115.00 Add to cart -
ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
0 out of 5CDN $76.00 Add to cart