REGISTER

FR
Search
×
FR

Placeholder headline

This is just a placeholder headline

API SPEC 14L: Lock Mandrels and Landing Nipples : Reaffirmed

$

273

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 20F: Corrosion Resistant Bolting for Use in the Petroleum and Natural Gas Industries : Reaffirmed

$

169

BUY NOW

Placeholder headline

This is just a placeholder headline

API TR 5NCL Nickel Content Limits for API 5CT Sour Service Products

$

149

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 19ICD: Inflow Control Devices : Reaffirmed

$

189

BUY NOW

Placeholder headline

This is just a placeholder headline

API MPMS CH 23.2: Reconciliation of Liquid Tank Car(s) Quantities : Reaffirmed

$

218

BUY NOW

Placeholder headline

This is just a placeholder headline

API SPEC 16A: Specification for Drill-through Equipment

$

322

BUY NOW

Placeholder headline

This is just a placeholder headline

API RP 13B-2: Field Testing Oil-based Drilling Fluids wA1

$

388

BUY NOW

ISO 9591:2004

ISO 9591:2004 Corrosion of aluminium alloys – Determination of resistance to stress corrosion cracking

CDN $115.00

Description

ISO 9591:2004 specifies a method for the determination of resistance to stress corrosion cracking (SCC) of aluminium alloys.

It covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.

This International Standard is aimed at determining resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of aluminium alloys.

It applies to cast and wrought aluminium alloys in the form of castings, semi-finished products, parts and weldments.

Since most natural and many artificial environments contain chlorides, ISO 9591:2004 can be used to compare the performance of products employed under marine atmospheres and in environments containing chlorides, providing that the failure mechanism is not changed.

Edition

2

Published Date

2004-09-13

Status

PUBLISHED

Pages

11

Language Detail Icon

English

Format Secure Icon

Secure PDF

Abstract

ISO 9591:2004 specifies a method for the determination of resistance to stress corrosion cracking (SCC) of aluminium alloys.

It covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.

This International Standard is aimed at determining resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of aluminium alloys.

It applies to cast and wrought aluminium alloys in the form of castings, semi-finished products, parts and weldments.

Since most natural and many artificial environments contain chlorides, ISO 9591:2004 can be used to compare the performance of products employed under marine atmospheres and in environments containing chlorides, providing that the failure mechanism is not changed.