API TR 13TR1: Stress Corrosion Cracking of Corrosion Resistant Alloys in Halide Brines Exposed to Ac
CDN $242.08
Description
To understand the effects of brine compositions on the CRAs, a joint industry project was formed under the auspices of the American Petroleum Institute (API). It has been known as the CRAs in Brine Testing Program. Under its auspices, work has been underway for a number of years on understanding the interaction of brine chemistry and CRAs. The current paper evaluates the SCC risks of a range of CRAs in various halide brine compositions for the case of exposure to acidic production gas (CO2+H2S). Also evaluated are SCC risks due to air exposure. However, the testing became focused on a group of martensitic stainless steels alloyed with Ni and Mo, that are collectively referred to as modified 13Cr martensitic SS, or alternatively in some publications as super (S13Cr) martensitic SSs. Most tests evaluated the as-received brine, excluding proprietary additives such as corrosion inhibitor or oxygen scavengers. For completeness and comparison, test results provided by member companies in the
Edition
1
Published Date
2017-11-14
Status
Current
Pages
39
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
To understand the effects of brine compositions on the CRAs, a joint industry project was formed under the auspices of the American Petroleum Institute (API). It has been known as the CRAs in Brine Testing Program. Under its auspices, work has been underway for a number of years on understanding the interaction of brine chemistry and CRAs. The current paper evaluates the SCC risks of a range of CRAs in various halide brine compositions for the case of exposure to acidic production gas (CO2+H2S). Also evaluated are SCC risks due to air exposure. However, the testing became focused on a group of martensitic stainless steels alloyed with Ni and Mo, that are collectively referred to as modified 13Cr martensitic SS, or alternatively in some publications as super (S13Cr) martensitic SSs. Most tests evaluated the as-received brine, excluding proprietary additives such as corrosion inhibitor or oxygen scavengers. For completeness and comparison, test results provided by member companies in the
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
API SPEC 10F: Cementing Float Equipment Testing
0 out of 5CDN $145.25 Add to cart -
API RP 10B-3: Testing of Well Cements Used in Deepwater Well Construction
0 out of 5CDN $185.31 Add to cart -
API TR 10TR3: Temperatures for API Cement Operating Thickening Time Tests
0 out of 5CDN $307.19 Add to cart -
API TR 10TR5: Technical Report on Methods for Testing of Solid and Rigid Centralizers
0 out of 5CDN $120.20 Add to cart