API TR 934-F, Part 3
API TR 934-F, Part 3: Subcritical Cracking of Modern 2-1/4Cr-1Mo-1/4V Steel Due to Dissolved-Interna
CDN $340.58
Description
This Technical Report conveys the results of API-sponsored research to: (a) quantitatively characterize the internal hydrogen assisted cracking (IHAC) resistance of modern 2¼Cr-1Mo-¼V steel, in both base metal and weld metal product forms and including the effect of stressing temperature, (b) scope the hydrogen environment assisted cracking (HEAC) resistance of 2¼Cr-1Mo-¼V base metal, (c) understand the mechanism(s) for the IHAC and HEAC behaviors of Cr-Mo and Cr-Mo-V steels, centered on H interactions with microstructure-scale trap sites, and (d) assess application of data and understanding of IHAC and HEAC to determine the role of subcritical H-assisted cracking on a minimum pressurization temperature estimate relevant to thick-wall hydro-treating reactor vessels. This work focuses on slow-stable subcritical H cracking, and did not examine the effect of H on the fracture toughness for unstable cracking. The temperature dependencies of internal hydrogen assisted cracking (IHAC) of
Edition
1
Published Date
2017-12-06
Status
Current
Pages
170
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This Technical Report conveys the results of API-sponsored research to: (a) quantitatively characterize the internal hydrogen assisted cracking (IHAC) resistance of modern 2¼Cr-1Mo-¼V steel, in both base metal and weld metal product forms and including the effect of stressing temperature, (b) scope the hydrogen environment assisted cracking (HEAC) resistance of 2¼Cr-1Mo-¼V base metal, (c) understand the mechanism(s) for the IHAC and HEAC behaviors of Cr-Mo and Cr-Mo-V steels, centered on H interactions with microstructure-scale trap sites, and (d) assess application of data and understanding of IHAC and HEAC to determine the role of subcritical H-assisted cracking on a minimum pressurization temperature estimate relevant to thick-wall hydro-treating reactor vessels. This work focuses on slow-stable subcritical H cracking, and did not examine the effect of H on the fracture toughness for unstable cracking. The temperature dependencies of internal hydrogen assisted cracking (IHAC) of
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
API SPEC 12D: Specification for Field Welded Tanks for Storage of Production Liquids
0 out of 5CDN $207.02 Add to cart -
API RP 2350: Overfill Prevention for Storage Tanks in Petroleum Facilities
0 out of 5CDN $242.08 Add to cart -
API RP 2003: Protection Against Ignitions Arising Out of Static, Lightning, and Stray Currents
0 out of 5CDN $370.63 Add to cart -
API RP 505: Recommended Practice for Classification of Locations for Electrical Installations at Pet
0 out of 5CDN $435.74 Add to cart