ISO 11463:2020 Corrosion of metals and alloys – Guidelines for the evaluation of pitting corrosion
CDN $115.00
SKU: 1f95f25c6f1d
Categories: ICS:77.060, SUSTAINABLE_DEVELOPMENT_GOAL:15, SUSTAINABLE_DEVELOPMENT_GOAL:6, SUSTAINABLE_DEVELOPMENT_GOAL:7
Description
This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.
Edition
2
Published Date
2020-08-06
Status
PUBLISHED
Pages
12
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 20670:2023 Water reuse – Vocabulary
0 out of 5CDN $173.00 Add to cart -
ISO 23066:2021 Vocabulary related to rattan materials and products
0 out of 5CDN $76.00 Add to cart -
ISO 41011:2024 Facility management – Vocabulary
0 out of 5CDN $233.00 Add to cart -
ISO 1956:1982 Fruits and vegetables – Morphological and structural terminology
0 out of 5CDN $233.00 Add to cart