ISO 7539:1989 Corrosion of metals and alloys – Stress corrosion testing – Part 5: Preparation and use of C-ring specimens
CDN $115.00
Description
Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.
Edition
1
Published Date
1989-12-07
Status
PUBLISHED
Pages
9
Format 
Secure PDF
Secure – PDF details
- Save your file locally or view it via a web viewer
- Viewing permissions are restricted exclusively to the purchaser
- Device limits - 3
- Printing – Enabled only to print (1) copy
See more about our Environmental Commitment

Abstract
Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.
Previous Editions
Can’t find what you are looking for?
Please contact us at:
Related Documents
-
ISO 5053:2019 Industrial trucks – Vocabulary – Part 2: Fork arms and attachments
0 out of 5CDN $351.00 Add to cart -
ISO 80004:2021 Nanotechnologies – Vocabulary – Part 6: Nano-object characterization
0 out of 5CDN $76.00 Add to cart -
ISO 2574:1994 Aircraft – Electrical cables – Identification marking
0 out of 5CDN $115.00 Add to cart -
ISO 80004:2020 Nanotechnologies – Vocabulary – Part 8: Nanomanufacturing processes
0 out of 5CDN $76.00 Add to cart